Table 3 Surface resistivity of samples coated with formulation A and B

From: Textile piezoelectric sensors – melt spun bi-component poly(vinylidene fluoride) fibres with conductive cores and poly(3,4-ethylene dioxythiophene)-poly(styrene sulfonate) coating as the outer electrode

Sample Coating A Coating B
Initial surface resistivity (Ω/square) 134 12.3
Surface resistivity after Martindale (50 000 cycles) (Ω/square) 171 74