Skip to main content

International Journal of Interdisciplinary Research

Fig. 1 | Fashion and Textiles

Fig. 1

From: Characterization of grafted jute fiber using acrylate monomers pretreated with alkali

Fig. 1

Plots of polymerization temperature vs percent graft yield where 80 % EA and 70 % HEMA as monomer, 4.5 % K2S2O8 for EA and 4 % K2S2O8 for HEMA as initiator, 5 % FeSO4 for EA and 4.5 % FeSO4 for HEMA as catalyst, 90 min reaction time for both EA and HEMA (graft yield: filled diamond bleached modified with EA, filled square alkali-activated bleached modified with EA, filled triangle bleached modified with HEMA and Times alkali-activated bleached modified with HEMA

Back to article page