Table 7 Bending length of treated and untreated samples

From: Sustainable approach for development of antimicrobial textile material using nanoemulsion for wound care applications

Test sample (%) Bending length (cm)a
Before finish After finish
0.5 4.3 4.8
0.3 3.8 4.2
0.1 3.6 4.0
  1. aBending length of control sample: 3.4