Table 2 Comparison of fabric properties between untreated and treated dyed cotton

From: Development of shrink resistance cotton using fluorocarbon

S. no.

Parameters

Untreated dyed fabric

Treated dyed fabric

1

Colour fastness to washing

 Change in colour

4 to 5

4 to 5

 Staining on adjacent fabric

4 to 5

4 to 5

2

Colour fastness to rubbing

 Staining on adjacent fabric

 Wet rubbing

4 to 5

4 to 5

 Dry rubbing

4 to 5

4 to 5

3

Colour fastness to perspiration

 Acidic

  Change in colour

4 to 5

4

  Staining on adjacent fabric

4 to 5

4 to 5

 Alkaline

  Change in colour

4 to 5

4 to 5

  Staining on adjacent fabric

4 to 5

4 to 5

4

Colour fastness to light

> 3

> 3

 Change in colour

5

Tensile strength (Newtons)

 Warp

256

236

 Weft

240

224

6

Tear strength (Newtons)

 Warp

37.85

35.10

 Weft

37.52

34.34