Fig. 10From: The effect of 10,12-pentacosadiynoic acid on the morphology and characteristics of electrospun PDA/PU nanofibersDiameter (nm) of nanofibers fabricated by electrospinning two different ratios of PU:PCDA (spinning solution concentration: 16 wt%)Back to article page