Table 3 Measured temperature rises after 20 min of heating

From: 3D-printed thermoplastic polyurethane for wearable breast hyperthermia

Infill (%) Solid volume (%) Temperature rise (°C) at 5 mm Temperature rise (°C) at 7 mm
70.0 82.4 5.5 3.2
100.0 100.0 5.6 3.3