Fig. 5From: Fabrication of polyester fabrics with tungsten bronze nanorods and a silane coupling agent for improved thermal storage and washing durabilityGraph of temperature change of PET samples with time (a) and NIR images (b) under white light irradiation for 1 h and after turning off the light for the following 15 minBack to article page