Fig. 3From: Development of shrink resistance cotton using fluorocarbonComparison of weft wise shrinkage of untreated (0 g/L) and treated cotton with fluorocarbon at 10 to 60  g/L. Weft-wise shrinkage of untreated and treated cottonBack to article page